Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.05 | 0.35 | 0.35 | 0.015 | 0.015 | 17-21 | 50-55 |
| Mo | Al | Cu | Nb | Ti | V | Ce |
| 2.8-3.3 | 0.2-0.8 | ≤0.3 | 4.75-5.25 | 0.65-1.15 | ||
| N | Co | Pb | B | Other | ||
| ≤0.01 | ≤1 | ≤0.006 | Fe... | |||
Click the Get Adobe Reader button to download the Adobe Reader:
Related steel grade search:INCONEL alloy 718 SPF
Previous pageINCONEL alloy 718