Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.07-0.15 | 0.5-0.8 | 1.5-2.0 | 0.025 | 0.035 | ||
| Mo | Al | Cu | Nb | Ti | V | Ce |
| ≤0.5 | ||||||
| N | Co | Zr | B | Other | ||
| Cr+Ni+Mo+V≤0.5% | ||||||