| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| 1.00-1.10 | 0.10-0.30 | 0.10-0.40 | 0.030 | 0.030 |