| Annealing | Quenching | Tempering | Normalizing | Q & T | 
| √ | √ | √ | √ | √ | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.73-0.83 | 0.45 | 0.4 | 0.03 | 0.03 | 3.8-4.5 | |
| Mo | Al | Cu | Nb | W | V | Ce | 
| 17.2-18.7 | 1.0-1.2 | |||||
| N | Co | Pb | B | Other | ||