Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.15-0.20 | 0.50-0.60 | 0.65-0.75 | 0.030 | 0.030 | 0.50-0.60 | 0.70-0.80 |
| Mo | Al | Cu | Nb | Ti | V | Ce |
| 0.60-0.70 | ||||||
| N | Co | Pb | B | Other | ||
Click the Get Adobe Reader button to download the Adobe Reader:
Related steel grade search:G17NiMoCr3-6